KelvinProbeForceMicroscopy Pinpoint Collagen HighResolution Anneal Worcester_Polytechnic_Institute TappingMode FloppyDisk mechanical property Ni81Fe19 medical silicon_carbide Silver Boron organic_polymer LightEmiting Lanthanum_aluminate Polyimide Piranha Dimethicone fluorocarbon Biology ScanningThermalMicroscopy LiquidCrystal EvatecAG Non-ContactMode StyreneBeads SoftSample InLiquid flakes ring shape mfm_amplitude SiliconeOxide SrTiO3 layers
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Ceramic Portland cement
Scanning Conditions
- System : NX10
- Scan Mode: Tapping
- Scan Rate : 1Hz
- Scan Size : 1μm×1μm
- Pixel Size : 256×256
- Cantilever : PPP-NCHR (k=42N/m, f=330kHz)