AM-KPFM Deposition molecular_self_assembly HexagonalBoronNitride polymeric_arrays PolymerBlend small_scan Domain TCS NusEce SKKU Chemical Vapor Deposition Potential Floppy aluminum_nitride Celebration PhthalocyaninePraseodymium HydroGel Bacteria PinPointMode Vacuum LateralForce Beads UnivOfMaryland AdhesionForce cross section Nanotechnology lithography SRAM EPFL KAIST pulsed_laser_deposition SrTiO3 Indium_tin_oxide OpticalWaveguide
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Margarines
Phase change of Margarine surface by temperature control
Scanning Conditions
- System: NX10
- Scan Mode: Tapping, TCS1
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1.2Hz
- Pixel Size: 256 × 256
- Scan Mode: Tapping, TCS1
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1.2Hz
- Pixel Size: 256 × 256