PolycrystallineFerroelectricBCZT Microchannel Modulus PhaseChange GlassTemperature sputter Fet FrictionForce LiquidImaging Aggregated_molecules Sio2 temp_control VinylAlcohol rubber Materials #EC Ananth Dopped Workfunction atomic_steps LightEmiting ConductingPolymer ThermalDetectors HexagonalBN Platinum GaAs cannabis Flake SolarCell OrganicSemiconductor SiliconeOxide self_healing Formamidinium_lead_iodide Terrace Typhimurium
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Alkane Film (C60H122)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm, 0.5μm×0.5μm
- Scan Rate: 0.8Hz, 0.8Hz
- Pixel: 512×512, 512×512
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm, 0.5μm×0.5μm
- Scan Rate: 0.8Hz, 0.8Hz
- Pixel: 512×512, 512×512