TriGlycineSulphate ForceVolumeImage CBD FM_SKPM NTU self_assembly 2-vinylpyridine LateralForceMicroscopy HumanHair Ferroelectric ScanningTunnelingMicroscopy BiVO4 Potential Moire Foil TyphimuriumBiofilm DeflectionOptics PtfeFilter PolymerBlend temperature controller AFM 3-hexylthiophene SiWafer Hole align cannabidiol Composite PpLdpe vertical_PFM norganic EFMAmplitude Zagreb Piezo Metal-organicComplex PinpointPFM Lanthanum_aluminate
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Styrene beads
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 0.5Hz
- Pixel: 512×512