HanyangUniv Resistance TungstenDeposition WWafer Cross-section Wildtype lithography PatternedSapphireSubstrat Solar Chemical_Vapor_Deposition ReflexLens Vacuum semifluorinated_alkane Magnets amplitude_modulation self_healing TemperatureControl FrequencyModulation ThermalConductivity Plug TemperatureControlledAFM self_assembly HfO2 Etch C36H74 domain_switching margarine Logo Corrosion HexagonalBN MembraneFilter Ferrite Optic high_resolution neodymium_magnets
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/LDPE
Scanning Conditions
- System : FX40
- Scan Mode: PinPoint nanomechanical
- Scan Rate : 0.15 Hz
- Scan Size : 50μm×50μm
- Pixel Size : 256×256
- Cantilever : OMCL-AC160TS (k=26N/m, f=300kHz)