3-hexylthiophene Temasek_Lab KevlarFiber dielectric_trench VortexCore MagneticArray cooling Ananth Grain Wonseok Al2O3 BoronNitride fe_nd_b #Materials epitaxy lithography Fendb Heat China INSPParis DomainSwitching SetpointMode Water CuParticle mechanical property Stiffness MultiferroicMaterials Graphite Friction MetalCompound Polydimethylsiloxane Composite Conductance DLaTGS GaN
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PP/LDPE polymer blend
Scanning Conditions
- System: NX20
- Scan Mode: Pinpoint mechanical
- Cantilever: FMR (k=2N/m, f=75kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.35Hz
- Pixel: 256×256
- Modulus calculation model: Hertzian