CaMnO3 Bismuth ImideMonomer GranadaUniv Silver Ni-FeAlloy lift_mode KevlarFiber FloppyDisk CuParticle Logo thermal_conductivity Mechanical&nanotechnology Vortex IndiumTinOxide PFM Heat TemperatureControllerStage atomic_steps Wildtype Sio2 suspended_graphene Polyurethane Chemical_Vapor_Deposition Device CeramicCapacitor Ferrite Hafnium_dioxide Tin sulfide UnivOfMaryland self_assembly ForceVolume CrossSection SiliconOxide INSPParis
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Collagen fibrils
Scanning Conditions
- System : NX10
- Scan Mode: Tapping in Liquid
- Scan Rate : ALL 0.3Hz
- Scan Size : 10μm2, 4μm2
- Pixel Size : ALL 256×256
- Cantilever : PPP-FMR (k=2.8N/m, f=75kHz)