IISCBangalore Fet pinpoint mode Workfunction lithography dielectric_trench Defect fifber SetpointMode vertical_PFM medical Heating ForceVolume ElectroChemical ImideMonomer PolymerPatterns FrictionForce NeodymiumMagnets SiWafer PolyvinylideneFluoride FuelCell Pore Iron Indium_tin_oxide Stiffness Nanotechnology LowDensityPolyethylene Molybdenum_disulfide Chloroform LiBattery Ram Inorganic_Compound IVSpectroscopy Melt Bmp
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Kevlar fiber
Scanning Conditions
- System: XE7
- Scan Mode: NCM, F/D mapping
- Cantilever: Diamond probe(k=151N/m, f=50kHz)
- Scan Size:15μm×15μm
- Scan Rate: 0.5Hz
- Pixel: 512×256
- Scan Mode: NCM, F/D mapping
- Cantilever: Diamond probe(k=151N/m, f=50kHz)
- Scan Size:15μm×15μm
- Scan Rate: 0.5Hz
- Pixel: 512×256