NUSNNI blended polymers cannabinoid VortexCore Polystyrene SSRM Fiber CarbonNanotube GaN NUS_Physics Varistor CompactDisk SFAs Au111 TemperatureControlledAFM Styrene MultiLayerCeramicCapacitor molecule Barium_titanate VerticalPFM Ni-FeAlloy Corrosion LightEmiting MfmAmplitude Thermal gallium_nitride Polytetrafluoroethylene #Materials plastic Moire Tungsten Copolymer WPlug epitaxy Aluminum
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Christmas ball lithography on Si substrate
Scanning Conditions
- System: NX10
- Scan Mode: Contact, lithography
- Cantilever: : ContscPt (k=0.2N/m, f=25kHz)
- Scan Size: 30μm×30μm
- Scan Rate: 0.5Hz
- Pixel: 512×512