GlassTemp ForceMapping polyvinyl acetate Ram LiftMode Sapphire Polydimethylsiloxane frequency_modulation Molybdenum_disulfide cannabidiol Ferrite BFO ForceVolumeMapping MoS2 Carbon Lateral_Force_Microscopy Metal ScanningKelvinProbeMicroscopy Indium_tin_oxide PDMS Conducting Conduct ScratchMode SmalScan Sidewall Composition Litho Solar Ecoli silicon_oxide TempControl WWafer domain_switching BlockCopolymer ConductingPolymer
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polymer blend with nanofiber
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel: 512×512
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel: 512×512