Composite hard_disk_media Alkane TyphimuriumBiofilm Hysteresys doped OpticalElement heterojunctions Led Phosphide self_healing Writing Temasek_Lab FM-KPFM cannabidiol Vinylpyridine Polyvinylidene_fluoride Film LiNbO3 Pyroelectric Dr.JurekSadowski Scratch PolycrystallineFerroelectricBCZT FrictionalForce Implant Epoxy mono_layer phase_change temp C36H74 Hexacontane Nanotechnology nanobar epitaxy Insulator
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Block copolymer ΙΙ
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm, 0.3μm, 0.1μm
- Scan Rate: 1Hz, 1Hz, 2Hz
- Pixel: 512×512, 256×256, 256×256
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm, 0.3μm, 0.1μm
- Scan Rate: 1Hz, 1Hz, 2Hz
- Pixel: 512×512, 256×256, 256×256