biocompatible Hafnium_dioxide F14H20 Steps Litho NUS Wonseok Polyvinylidene semifluorinated_alkanes Semiconductor Implant Collagen blended polymers Piranha light_emitting organic_polymer thermal_property PinPointMode CNT Fluoride CarbonNanotube fluorocarbon Lanthanum_aluminate HACrystal HafniumDioxide SThM FAFailureAnlaysis Writing CBD Chungnam_National_University amplitude_modulation EFMAmplitude CeramicCapacitor India BloodCell
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Gold(111) coated mica substrate
Scanning Conditions
- System: XE7
- Scan Mode: Contact
- Cantilever: PPP-ContScR (k=0.2N/m, f=25kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel: 256×256
- EC electrode: Ag/AgCl2(Reference electrode), Pt(Counter electrode), CuSO4(0.1mM) + H2SO4(0.01mM)(Electrolyte)
- EC bias voltage: -0.3V