lithography lift_mode Piezoresponse Hexatriacontane LogAmplifier PtfeMembrane Worcester_Polytechnic_Institute DNAProtein Zagreb Bmp ForceVolumeImage Liquid Granada CuFoil Plug Writing Epoxy PolycrystallineFerroelectricBCZT cross section GaN SiWafer IcelandSpar Friction temperature controller AFM Strontium PolymerPatterns PhaseTransition temperature_control AlkaneFilm AM_KPFM Bismuth MolybdenumDisulfide Ucl Organic Conducting
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Calcium Hydroxyapatite Crystal growing
HA crystal grows according to the annealing time. From 24hrs, the crystal becomes clearly.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.17Hz
- Pixel: 512×256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.17Hz
- Pixel: 512×256