Fiber PDMS MagneticPhase IRDetector Singapore ConductingPolymer mfm_amplitude Jason HumanHair Wonseok Semiconductor dielectric trench Photovoltaics Plug Magnetic Bacteria BloodCell MultiferroicMaterials Gallium_Arsenide Step Logo India FrequencyModulation biocompatible LightEmiting SrTiO3 kelvin probe force microscopy LFM FM-KPFM Bacterium Leakage BaTiO3 Materials Lattice MechanicalProperty
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
NiFe
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 1.2μm×1.2μm
- Scan Rate: 0.5Hz
- Pixel: 256×256
- Lift height: 20nm
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 1.2μm×1.2μm
- Scan Rate: 0.5Hz
- Pixel: 256×256
- Lift height: 20nm