Mechanical Indium_tin_oxide Oxidation MembraneFilter PatternedSapphireSubstrat Reduction LMF conductive Sadowski ConductingPolymer Pinpoint #EC Growing AdhesionEnergy LateralForceMicroscopy NTU Organic PyroelectricDetector UnivMaryland C_AFM Sapphire AM_KPFM TriGlycineSulphate Layer Phosphide YszSubstrate 2dMaterials Thermoplastic_polyurethane InsulatorFilm HardDiskMedia PolyvinylAcetate Electronics Photovoltaics Magnetic Force Microscopy Foil
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Li ion battery electrode
Scanning Conditions
- System: NX-Hivac
- Scan Mode: SSRM
- Cantilever: CDT-NCHR (k=80 N/m)
- Scan Size: 50μm×50μm
- Scan Rate: 1Hz
- Pixel: 4096×2048