Neodymium LifeScience LMF TemperatureControlledAFM Pinpoint PFM PolyimideFilm 2dMaterials Sphere nanomechanical Ferrite Hafnium_dioxide Litho temperature_control FrictionalForce Austenite DNA ShenYang GalliumPhosphide Chrome FailureAnalysis SPMLabs Tungsten ForceMapping ElectroChemical Piezoelectric HardDiskMedia Roughness Sadowski PUR HfO2 HighAspect CHRYSALIS_INC HighAcpectRatio molecular_beam C_AFM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PZT thin film
Scanning Conditions
- System: NX10
- Scan Mode: PFM (DC-EFM)
- Cantilever: ContscPt (k=0.2N/m, f=25kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 0.5Hz
- Pixel: 512×512