UnivCollegeLondon Implant Roughness MolecularSelfAssembly Aluminium_Oxide SiliconCrystal CrAu tip_bias_mode MagneticForce ULCA FFM BiFeO3 mechanical property Vac Nanopattern CalciumHydroxide Leakage ShenYang Glass ItoGlass Worcester_Polytechnic_Institute Flake Polyaniline semifluorinated alkane molecules MagneticForceMicroscopy Adhesive Hysteresys CuParticle Collagen HDD OrganicCompound CastIron Grain Ptfe
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Red Blood Cell
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: ACTA (k=40N/m, f=300kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel: 256×256