StyreneBeads Resistance LaAlO3 ThinFilm alkanes ForceDistanceSpectroscopy StrontiumTitanate StrontiuTitanate ScanningTunnelingMicroscopy ImideMonomer UnivMaryland Ca10(PO4)6(OH)2 Kevlar FrictionalForce Device Magnetostrictive Ucl small_scan Lattice Vanadate Polymer Scanning_Thermal_Microscopy Galfenol Wafer Pore ChemicalCompound Modulus Hafnia BlockCopolymer Alloy KelvinProbeForceMicroscopy PUR Materials organic_polymer optoelectronics
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Perovskite coated on glass with Palladium electrodes
Scanning Conditions
- System : FX40
- Scan Mode: Sideband KPFM
- Scan Rate : All 0.4 Hz
- Scan Size : 40μm×40μm
- Pixel Size : All 256×256
- Cantilever : NSC36 Pt C(k=0.6N/m, f=65kHz)