Perovskite BariumTitanate Pyroelectric PvdfBead Varistor medical TPU PUR Tungsten_disulfide gallium_nitride Pattern BoronNitride Mechanical&nanotechnology Corrosion Laser membrane LFM MfmAmplitude nanomechanical Roughness GalliumPhosphide TiO2 SetpointMode C_AFM CaMnO3 hard_disk Domain Ferrite ConductingPolymer self-assembly Patterns PolycrystallineFerroelectricBCZT TCS Oxidation Magnetic
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Semi-fluorinated alkanes
Scanning Conditions
- System : NX10
- Scan Mode: Sideband KPFM
- Scan Rate : 0.4 Hz
- Scan Size : 500nm×500nm
- Pixel Size : 256×256
- Cantilever : HQ: NSC14/CR-AU (k=5N/m, f=160kHz)