Ni81Fe19 FrequencyModulation BiasMode Litho Etch cooling Dental DomainSwitching PinPointMode LightEmiting ScanningThermalMicroscopy InsulatorFilm Tape Film KevlarFiber Granada Pinpoint SmallScan Molybdenum_disulfide hard_disk Pipette Ram Sulfur LiquidCell BaTiO3 PFM StrontiuTitanate Ecoli SICM CalciumHydroxyapatite China F14H20 Phenanthrene Polymer bias_mode
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Escherichia coi (E. coli)
Scanning Conditions
- System : NX10
- Scan Mode: Non-contact
- Scan Rate : 0.5 Hz
- Scan Size : 20μm×20μm
- Pixel Size : 256×256
- Cantilever : PPP-NCHR (k=42N/m, f=330kHz)