PVAC Conductance Current Forevision hetero_structure DeoxyribonucleicAcid HBN ScanningThermalMicroscopy DIWafer Chungnam_National_University ElectroChemical LaAlO3 PhthalocyaninePraseodymium Fujian KAIST Ferrite NUS_NNI_Nanocore CalciumHydroxide ForceDistanceSpectroscopy layers Epoxy Tungsten_disulfide H-BN MultiferroicMaterials Polypropylene atomic_layer Adhesion VerticalPFM ConductiveAFM Melt Graphene Pores WWafer LFM VortexCore
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Nanostructures on polymer
Scanning Conditions
- System : NX10
- Scan Mode: Non-contact
- Scan Rate : 0.5 Hz
- Scan Size : 5μm×5μm
- Pixel Size : 256×256
- Cantilever : PPP-NCHR (k=42N/m, f=330kHz)