atomic_steps VinylAlcohol YszSubstrate hetero_structure Imprint Annealing LogAmplifier Chromium WWafer Tungsten MoS2 Chemical_Vapor_Deposition Mfm TransitionMetal NCM DeoxyribonucleicAcid strontiu_titanate FrictionalForce Celebration Formamidinium_lead_iodide Nanotechnology AAO OrganicCompound MetalCompound Ptfe Beads Sidewall SurfaceOxidation HighResolution HafniumDioxide TempControl LateralForceMicroscopy ForceVolumeMapping plastic ElectroChemical
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PMN-PT single crystal
Scanning Conditions
- System: NX10
- Scan Mode: PFM
- Cantilever: NSC36A Ti-Pt (k=1N/m, f=90kHz)
- Scan Size: 8μm×8μm
- Scan Rate: 0.5Hz
- Pixel: 512×256