OxideLayer single_layer Optoelectronic Electrode electrospinning Styrene tip_bias_mode PS_PVAC Polyvinylidene Perovskite plastic CntFilm Piranha Annealing PetruPoni_Institute ContactModeDot dichalcogenide ThermalConductivity ImideMonomer LiftMode Switching plastics InLiquid C36H74 2d_materials ForceVolumeImage GlassTemperature Carbon Conductance P3HT block_copolymer Croatia Typhimurium Worcester_Polytechnic_Institute SingleLayer
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Al2O3-doped CaMnO3
1% Al2O3-doped CaMnO3 on LaAlO3 (001) orientation substrate by pulsed laser deposition.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256