KAIST IcelandSpar Tungsten Formamidinium_lead_iodide Composition kelvin probe force microscopy Sapphire #Materials PVA ring shape PhaseTransition Nanotechnology HumanHair Multiferroic_materials Annealed Ram TappingMode GalliumPhosphide Pipette PVAP3HT NeodymiumMagnets ContactModeDots HexacontaneFilm Photovoltaics Mfm Device StyreneBeads SmallScan LateralForce StainlessSteel Mapping Writing LDPE UnivCollegeLondon LateralPFM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Hard Disk Media
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: SSS-NCHR (k=42N/m, f=300kHz)
- Scan Size: 1μm×1μm, 0.3μm×0.3μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel Size: 512×512, 256×256
- Scan Mode: Non-contact
- Cantilever: SSS-NCHR (k=42N/m, f=300kHz)
- Scan Size: 1μm×1μm, 0.3μm×0.3μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel Size: 512×512, 256×256