Defect DeflectionOptics pulsed_laser_deposition BloodCell Fet frequency_modulation Change Resistance Cobalt-dopedIronOxide Austenite Pattern TransitionMetal PS_LDPE Worcester_Polytechnic_Institute Spain 3-hexylthiophene PetruPoni_Institute pinpoint mode dielectric trench UnivCollegeLondon FrequencyModulation FuelCell fifber silicon_carbide small_scan contact SrO Logo LiquidCell Cell SurfaceChange Wildtype Biofilm PvdfBead MagneticForceMicroscopy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Calcite surface change in Ca(OH)2
Scanning Conditions
- System: NX20
- Scan Mode: Universal liquid cell, Contact mode
- Cantilever: BL-AC40TS
- Scan Size: 45μm×45μm, 0.5μm×0.5μm
- Scan Rate: 3Hz
- Sample: Iceland spar (calcite)
- React Solution Ca(OH)2
- Pixel: 512 × 256, 256 × 256
- Scan Mode: Universal liquid cell, Contact mode
- Cantilever: BL-AC40TS
- Scan Size: 45μm×45μm, 0.5μm×0.5μm
- Scan Rate: 3Hz
- Sample: Iceland spar (calcite)
- React Solution Ca(OH)2
- Pixel: 512 × 256, 256 × 256