Electronics HOPG Topography IcelandSpar CeNSE_IISc suspended_graphene Foil Crystal single_layer pulsed_laser_deposition Nickel HydroGel CuSubstrate Molybdenum_disulfide ferromagnetic Reading OpticalModulator ThermalProperties Domain CopperFoil Magnetic Force Microscopy Bio Resistance Electrical&Electronics cannabis Implant oxide_layer MechanicalProperty Nanopattern HexagonalBN KPFM Hafnia rubber Semiconductor Stiffness
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Lithography on compact disk
Scanning Conditions
- System: NX10
- Scan Mode: XEL
- Cantilever: NCHR (k=42N/m, f=300kHz)
- Scan Size: 7.5μm×7.5μm
- Scan Rate: 0.5Hz
- Pixel: 256×256
- Scan Mode: XEL
- Cantilever: NCHR (k=42N/m, f=300kHz)
- Scan Size: 7.5μm×7.5μm
- Scan Rate: 0.5Hz
- Pixel: 256×256