Jason BismuthVanadate Switching Vanadate Sapphire DeflectionOptics 2-vinylpyridine Yttria_stabilized_Zirconia heterojunctions SmalScan Scratch Litho StrontiumTitanate Magnetic Ca10(PO4)6(OH)2 Annealed Polyimide Array NeodymiumMagnets Spincast Yeditepe Deposition LifeScience Kevlar Croatia VinylAlcohol EFM PVAP3HT ImideMonomer 2d_materials Battery Cell Zagreb TempControl PDMS
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Block copolymer ; Fast scan
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC55TS (k=85N/m, f=1600kHz)
- Scan Size: 0.5μm×0.5μm
- Scan Rate: 6Hz, 13Hz
- Pixel: 256×256
- Scan Mode: Tapping
- Cantilever: AC55TS (k=85N/m, f=1600kHz)
- Scan Size: 0.5μm×0.5μm
- Scan Rate: 6Hz, 13Hz
- Pixel: 256×256