SrO Metal Polytetrafluoroethylene vertical_PFM EFMAmplitude AdhesionForce ForceMapping Dental optoelectronics OpticalWaveguide TungstenDeposition polyvinyl acetate thermal_property MetalCompound ConductiveAFM hard_disk BariumTitanate CrossSection doped Layer Tapping Gong BiasMode LifeScience Implant MoirePattern Dopped Edwin biocompatible Change PhthalocyaninePraseodymium Electical&Electronics CNT suspended_graphene CP-AFM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Co coated surface
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.7Hz
- Pixel: 512×256
- Lift height: 30nm
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.7Hz
- Pixel: 512×256
- Lift height: 30nm