LDPE MfmAmplitude C_AFM CuParticle SSRM GaAs Mfm FAPbI3 Corrosion CalciumHydroxide Polarization membrane Fe_film kelvin probe force microscopy Silicon mechanical property YszSubstrate Croatia PolyvinylAcetate Dopped Nanofiber PpLdpe BismuthFerrite ferromagnetic HardDisk SurfaceChange Semiconductor Ananth SAM Phenanthrene I-VSpectroscopy OrganicSemiconductor lift_mode Mechanical&nanotechnology ConductiveAFM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Stitched image of chiplet
Scanning Conditions
- System : NX-Wafer
- Scan Mode: Non-contact
- Scan Rate : 0.5 Hz
- Scan Size : 100μm×100μm for single image (200μm×200μm stitched image)
- Pixel Size : 512×128 for single image
- Cantilever : OMCL-AC240TS (k=2N/m, f=70kHz)