MoirePattern #EC MagneticArray Graphite Protein CuParticle BCZT chemical_compound SFAs Memory DeflectionOptics HBN INSP Polyethylene InorganicCompound WWafer exfoliate HiVacuum Ananth HighResolution ContactModeDots Austenite GranadaUniv Workfunction Resistance EvatecAG 2d_materials Calcium Wonseok Polypropylene Change Galfenol Alloy Water Inorganic
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Diamond with plated / gold nickel
Scanning Conditions
- System : NX20
- Scan Mode: Non-contact
- Scan Rate : 0.49 Hz for 30μm2, 4μm2 / 0.6 Hz for 2.25m2
- Scan Size : 30μm2, 2.25μm2, 4μm2
- Pixel Size : All 256×256
- Cantilever : AD-2.8-AS (k=2.8N/m, f=75kHz)