Strontium NiFe Piezo Implant LiftMode Plug HexacontaneFilm IndiumTinOxide SurfaceOxidation HexagonalBoronNitride FM-KPFM Topography DataStorage Spincast solar_cell CeNSE_IISc ForceVolumeImage Cross-section oxide_layer cannabis Modulus DiffractiveOpticalElements InLiquid phase_change bias_mode Phthalocyanine PhaseChange Techcomp mechanical_property Beads KelvinProbeForceMicroscopy Vac Display Reading Chrome
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
F14H20
Semifluorinated alkanes on Si.
Scanning Conditions
- System: NX10
- Scan Mode: AM-KPFM
- Cantilever: qpBioAC AuCB1 (k=0.3N/m, f=90kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 256
- Scan Mode: AM-KPFM
- Cantilever: qpBioAC AuCB1 (k=0.3N/m, f=90kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 256