Alkane Writing Indium_tin_oxide Chungnam_National_University Polyvinylidene SurfaceOxidation ScratchMode CopperFoil MBE Worcester_Polytechnic_Institute Polyaniline LateralForce InsulatorFilm cannabidiol #EC hetero_structure Sphere Scratch Leakage Mechinical dielectric_trench ForceVolumeImage Pinpoint PFM HardDiskMedia nanomechanical C36H74 ScanningIon-ConductanceMicroscopy Switching Barium_titanate CalciumHydroxide MembraneFilter mechanical_property FailureAnlaysis Metal Piezoresponse
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Self-assembly of Semi-fluorinated Alkanes
Domains formed by the self-assembly of semi-fluorinated alkanes deposited as a monolayer on the surface of the water. The monolayer was compressed before being transferred onto a silicon substrate. Each domain includes about 4000 molecules. The domains were easily detached from the substrate with tapping mode because the molecules were very loosely attached to the substrate. Only Non-contact mode could achieve this result.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: PPP-FMR (k=2.8N/m, f=75kHz)
- Scan Size: 1μm×1μm, 0.5μm×0.5μm, 0.2μm×0.2μm
- Scan Rate: 2Hz
- Pixel Size: 500 × 500
- Scan Mode: Non-contact
- Cantilever: PPP-FMR (k=2.8N/m, f=75kHz)
- Scan Size: 1μm×1μm, 0.5μm×0.5μm, 0.2μm×0.2μm
- Scan Rate: 2Hz
- Pixel Size: 500 × 500