Boundary CompactDisk PetruPoni_Institute BiasMode Plug PhaseChange DLaTGS Transparent GranadaUniv Gallium_Arsenide University_of_Regensburg SolarCell Moire lithography SThM HexagonalBoronNitride Aluminum Croatia rubber AEAPDES PvdfFilm Monisha non_contact doped Sic India Wildtype SmallScan Collagen ConductiveAFM CntFilm IIT-chennai Carbon semifluorinated_alkanes Polydimethylsiloxane
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polymer (2/2)
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: NCHR
- Scan Size:1μm×1μm
- Scan Rate: 1Hz
- Pixel: 256 × 256
- Scan Mode: Tapping
- Cantilever: NCHR
- Scan Size:1μm×1μm
- Scan Rate: 1Hz
- Pixel: 256 × 256