| お問い合わせ

Thickness maps of thin films on the water surface by imaging ellipsometry

SAMPLE AND SETUP:

 

The water surface is of elementary interest as well in biophysics as in industrial applications. Brewster Angle microscopy is state of the are in label free imaging of the water surface but enable only an estimation of layer thicknesses.

app05 fig02 new

To measure the thickness of ultra thin films, imaging ellipsometry is the method of choice and the nanofilm_EP4 can also be operated as a Brewster angle microscope. To Avoid the disturbents by vibration, an sufficticated anti vibration concept based on active vibrations isolation is requiered.

 

MEASUREMENT:

app29 fig01

Droplets of a Ethyl-stearate (1 mg/ml in Hexane) were spread with a microliter syringe at a cleaned water surface. Microscopic Delta and Psi maps were recorded with an single wave imaging ellipsometer equipped with a red laser (IEEP4L658nm) and a 5x objective. The instrument was mounted on an active vibration isolation system (Halcyonics_vario40). A round Teflon trough equipped with a wedge shaped black glass plate was set on top of a table top active vibration isolation system (halcyonics _nano20).

 

 RESULTS:

 

- microscopic Δ, Ψ maps

- Thickness maps on water

app29 fig02

app29 fig03