OpticalWaveguide Jason PtfeFilter fluoroaalkane Hydroxyapatite Optoelectronic CrystalGrowing graphene_hybrid VinylAlcohol Fluoride Electrical&Electronics margarine LiquidCrystal thermal_conductivity IIT-chennai Growing DataStorage Blend Hafnia Forevision ForceMapping PvdfBead Formamidinium_lead_iodide LogAmplifier Defects Conducting Ferroelectric ScanningTunnelingMicroscopy Copolymer HDD silicon_oxide PhthalocyaninePraseodymium SelfAssembly Silicon Adhesive
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Mechanical Exfoliated WS2
Scanning Conditions
- System: NX10
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au A (k=1N/m, f=90kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.4Hz
- Pixel: 512 × 256
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au A (k=1N/m, f=90kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.4Hz
- Pixel: 512 × 256