Nanotechnology PetruPoni Indent Perovskite ForceMapping Anneal kelvin probe force microscopy Heating DOE CHRYSALIS_INC ImideMonomer Array MfmAmplitude IMT_Bucharest food PinpointNanomechanicalMode Iron Worcester_Polytechnic_Institute FM_SKPM FailureAnalysis Optic ElectrostaticForceMicroscopy FAFailureAnlaysis Sidewall semifluorinated_alkanes FloppyDisk CuSubstrate FailureAnlaysis high_resolution Vanadate aluminum_nitride Deposition FastScan BloodCell LogAmplifier
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Atomic steps on STO(110)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: PPP-NCHR (k=42N/m, f=300kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.62Hz
- Pixel: 512×512