Yttria_stabilized_Zirconia DataStorage Galfenol CP-AFM Crystal Fiber Polyaniline Mechinical multi_layer FastScan Ni-FeAlloy YszSubstrate C36H74 Yeditepe_University Ecoli FrictionForce phase_change temp_control bias_mode Solution F14H20 Etch Reading Titanate NtuEee FrictionalForce KPFM Austenite ferromagnetic PhthalocyaninePraseodymium PetruPoni Corrosion SurfaceChange GranadaUniv Temperature
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Gold(111) coated mica substrate
Scanning Conditions
- System: XE7
- Scan Mode: Contact
- Cantilever: PPP-ContScR (k=0.2N/m, f=25kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel: 256×256
- EC electrode: Ag/AgCl2(Reference electrode), Pt(Counter electrode), CuSO4(0.1mM) + H2SO4(0.01mM)(Electrolyte)
- EC bias voltage: -0.3V