ConductingPolymer MembraneFilter LiquidImaging ScanningSpreadingResistanceMicroscopy Collagen PatternedSapphireSubstrat Vortex Copolymer MechanicalProperties Pattern fluoroalkane SiliconCrystal RedBloodCell HBN AdhesionForce TemperatureControl FrictionalForce PhaseTransition IcelandSpar ShenYang PvdfBead Device BismuthFerrite Domain ScratchMode Lateral_Force_Microscopy Ecoli CNT Gold YszSubstrate ThermalConductivity cannabinoid Mfm InsulatorFilm Ananth
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Li stripping-plating on Li surface
Scanning Conditions
- System : NX10 in dry room
- Scan Mode: Contact/EC AFM
- Scan Rate : 0.15 Hz
- Scan Size : 30μm×30μm
- Pixel Size : 256×256
- Cantilever : Multi75-G
- ECr : Li metal (Working electrode), Li metal (Reference electrode), Li (Counter electrode), 1M LiTFSI in TEGDME (Electrolyte)
- Open circuit voltage : 1 VLi/Li+