HafniumDioxide CaMnO3 HfO2 Treatment PetruPoni Vinylpyridine LiftHeight Phenanthrene Switching SRAM Ucl optoelectronics LDPE SiliconOxide Current Conductivity BiFeO3 MagneticForceMicroscopy FloppyDisk Dopped BloodCell Defects thermoplastic_elastomers Materials InsulatorFilm Holes dielectric_trench PiezoelectricForceMicroscopy Nanopattern SiWafer ConductingPolymer Dimethicone I-VSpectroscopy food WWafer
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Single-crystal SrTiO3(001) after Annealing
Single-crystal SrTiO3(001) after 1h annealing at 1000°C in air. Formation of steps and terraces, and assembly at the nanoscale of SrO and TiO2 chemical terminations.
Scanning Conditions
- System: NX10
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256