mfm_amplitude Anneal non_contact Change FFM biocompatible Dental Conductance semifluorinated_alkanes OpticalWaveguide SKKU VortexCore molecule Platinum Ram IIT-chennai Mechinical Barium_titanate PVAC Ucl block_copolymer Fiber Nanopattern SFAs STO CuSubstrate SKPM silicon_carbide ScanningTunnelingMicroscopy PetruPoni Non-ContactMode membrane sputter OrganicSemiconductor Biofilm
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/LDPE
Spincast layer of PS/LDPE blend on Si.
Scanning Conditions
- System: NX10
- Scan Mode: LFM
- Cantilever: BL-AC40TS (k=0.09N/m, f=110kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 512
- Scan Mode: LFM
- Cantilever: BL-AC40TS (k=0.09N/m, f=110kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 512