MembraneFilter StrontiuTitanate Phase OpticalWaveguides PetruPoni_Institute Piranha KevlarFiber Blend hetero_structure PFM Vinylpyridine CNT HDD block_copolymer Grain Chloroform SingleLayer MoirePattern Sic chemical_compound AtomicSteps SiliconOxide Hexacontane Electrical&Electronics PVA StainlessSteel Polystyrene TyphimuriumBiofilm HafniumDioxide Perovskite KelvinProbeForceMicroscopy Formamidinium_lead_iodide PMNPT PtfeFilter Polytetrafluoroethylene
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ER 316L Stainless Steel
The ferrite MFM phase has a striped appearance due to its ferromagnetic behavior, while the paramagnetic austenite phase shows a uniform appearance.
Scanning Conditions
- System: NX20
- Scan Mode: AM-KPFM, MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 512
- Lift height: 30nm
- Scan Mode: AM-KPFM, MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 512
- Lift height: 30nm