Mechanical&nanotechnology SelfAssembly Polystyrene Scratch MechanicalProperty FrictionForce Chemical_Vapor_Deposition PinpointNanomechanicalMode Blood Chrome Trench TemperatureControllerStage LifeScience PolymerPatterns HighAspect University_of_Regensburg Au111 DentalProsthesis Magnetic Force Microscopy FrequencyModulation EFM ItoGlass AlkaneFilm molecular_self_assembly bias_mode temperature controller AFM electrospinning pulsed_laser_deposition OpticalWaveguides Nickel PtfeMembrane MultiLayerCeramicCapacitor ForceDistanceSpectroscopy HDD Yeditepe
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
CVD Grown WS2
Scanning Conditions
- System: NX10
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au A (k=1N/m, f=90kHz)
- Scan Size: 17μm×17μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 256
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au A (k=1N/m, f=90kHz)
- Scan Size: 17μm×17μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 256