Molybdenum Indium_tin_oxide Lateral Permalloy Oxide Semiconductor Layer DiffractiveOpticalElements ScanningIon-ConductanceMicroscopy fifber BiVO4 AM_SKPM ContactModeDots TungstenDeposition Electronics PolyvinylAcetate BiFeO3 cannabis NCM\ Temperature VinylAlcohol Conducting Styrene pinpoint mode StainlessSteel NUS_Physics MagneticForceMicroscopy DNA Growing Zagreb molecular_beam Fiber Aluminium_Oxide Battery sputter
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Cast Iron surface change after Corrosion
Scanning Conditions
- System: NX10
- Scan Mode: Contact
- Cantilever: NSC36C (k=0.6N/m, f=65kHz)
- Scan Size: 50μm×50μm
- Scan Rate: 1.5Hz
- Pixel: 512×1024
- EC bias voltage: -0.266V