FM-KPFM Wang MagneticPhase Dental suspended_graphene DeflectionOptics TriGlycineSulphate Aluminum KevlarFiber Morphology Fet Ni-FeAlloy BloodCell Corrosion Collagen CuFoil piezoelectric force microscopy Perovskite AM_KPFM Tape Formamidinium_lead_iodide STO Flake Cobalt Modulus Chloroform IVSpectroscopy LiquidCrystal WWafer INSP frequency_modulation CalciumHydroxide 2dMaterials MembraneFilter Blend
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Hair
Scanning Conditions
- System: NX10
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au (k=0.6N/m, f=65kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.3Hz
- Pixel: 512×256