Layer oxide_layer MagneticForce IRDetector TungstenThinFilmDeposition Grain FrictionalForceMicroscopy SRAM LithiumNiobate Mechanical TCS Ito Reading Mosfet Galfenol ScanningSpreadingResistanceMicroscopy Floppy PolyStylene Sidewall Piezoelectric C60H122 UnivOfMaryland China Piranha Domain LDPE Sadowski Electronics IIT-chennai Pores SrTiO3 STO Nanostructure NTU piezoelectric force microscopy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
F14H20
Semifluorinated alkanes on Si.
Scanning Conditions
- System: NX10
- Scan Mode: AM-KPFM
- Cantilever: qpBioAC AuCB1 (k=0.3N/m, f=90kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 256
- Scan Mode: AM-KPFM
- Cantilever: qpBioAC AuCB1 (k=0.3N/m, f=90kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 256