suspended_graphene NiFe Conductance solar_cell Nanostructure Tin sulfide Protein CalciumHydroxyapatite silicon_carbide FM-KPFM FailureAnlaysis TappingMode Vac Ucl Patterns Au111 PS_LDPE WWafer PFM ferromagnetic PvdfFilm mechanical property Blend LogAmplifier hydrocarbon Ecoli HfO2 exfoliate Film TransitionMetal atomic_steps atomic_layer LowDensityPolyethylene Roughness LateralPFM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
CVD Grown WS2
Scanning Conditions
- System: NX10
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au A (k=1N/m, f=90kHz)
- Scan Size: 17μm×17μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 256
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au A (k=1N/m, f=90kHz)
- Scan Size: 17μm×17μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 256