Heat Genetic CeramicCapacitor Bismuth Reduction ForceDistanceSpectroscopy lift_mode BiasMode Leakage Nanofiber neodymium_magnets Change VortexCore Melt Chromium YszSubstrate Treatment Sio2 AlkaneFilm HACrystal strontiu_titanate PMNPT ConductingPolymer Dimethicone HexacontaneFilm FailureAnlaysis Iron Yeditepe PUR C36H74 Lanthanum_aluminate Defect LogAmplifier Implant Ecoli
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Al2O3-doped CaMnO3
1% Al2O3-doped CaMnO3 on LaAlO3 (001) orientation substrate by pulsed laser deposition.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256