Edwin Liquid Conductivity ThermalDetectors Fet ConductiveAFM temp_control Potential domain_switching Hexatriacontane GaAs InLiquid CompactDisk Hysteresys Forevision Epoxy C_AFM SurfaceChange MolybdenumDisulfide cannabis CBD ForceVolumeMapping VerticalPFM C60H122 Reduction atomic_steps Hexacontane HexagonalBoronNitride YszSubstrate Nanotechnology Imprint PolyvinylideneFluoride BariumTitanate Anneal FAPbI3
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Collagen film phase change by temp
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS
- Scan Size: 20μm×20μm, 1μm×0.5μm
- Scan Rate: 0.3Hz for 20µm×20µm scan, 1Hz for 1µm×0.5µm scan
- Pixel: 512 × 256 for 20µm×20µm scan, 256 × 128 for 1µm×0.5µm scan
- Scan Mode: Tapping
- Cantilever: AC160TS
- Scan Size: 20μm×20μm, 1μm×0.5μm
- Scan Rate: 0.3Hz for 20µm×20µm scan, 1Hz for 1µm×0.5µm scan
- Pixel: 512 × 256 for 20µm×20µm scan, 256 × 128 for 1µm×0.5µm scan