OpticalElement Sidewall biocompatible fifber BoronNitride Defect Au111 Electrode OpticalWaveguide cannabidiol SetpointMode mono_layer InorganicCompound Blend MoirePattern Phthalocyanine Yttria_stabilized_Zirconia Global_Comm INSP MembraneFilter Silicon NtuEee University_of_Regensburg Magnetostrictive Potential AmplitudeModulation SicMosfet NUS_NNI_Nanocore blended polymers hydrocarbon molecular_self_assembly NTU SiliconeOxide Wafer Typhimurium
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polyurethane
Scanning Conditions
- System: NX20
- Scan Mode: Non-contact, TCS
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel: 512×256