Praseodymium DeflectionOptics Ca10(PO4)6(OH)2 GlassTemp MagneticForce Nanofiber CeNSE_IISc PolyimideFilm Tape StrontiuTitanate Adhesion Led Layer Tin sulfide BFO MfmAmplitude Kevlar Chromium Biofilm Mechanical&nanotechnology ContactModeDots hydrocarbon LDPE Magnetic Force Microscopy BlockCopolymer Roughness Defects TPU AlkaneFilm StyreneBeads mono_layer Subhajjit Ni-FeAlloy LightEmiting Fluoride
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HOPG Moire
Scanning Conditions
- System: NX10
- Scan Mode: STM
- Cantilever: Pt wire
- Scan Size: 2.5μm×2.5μm, 0.5μm×0.5μm, 0.2μm×0.2μm
- Scan Rate: 0.3Hz, 1Hz, 2Hz
- Pixel: 512×256, 512×256, 256×128
- Scan Mode: STM
- Cantilever: Pt wire
- Scan Size: 2.5μm×2.5μm, 0.5μm×0.5μm, 0.2μm×0.2μm
- Scan Rate: 0.3Hz, 1Hz, 2Hz
- Pixel: 512×256, 512×256, 256×128